Characteristics:
- Low iron oxide content
- Low thermal conductivity
Application:
- Hot face lining
- Back up insulation
- Reducing atmosphere furnace
Classification temperature | 1550oC |
Recommended interface temperature | 1550oC |
Recommended hot face temperature | 1250 oC - 1450oC |
ASTM | SPECIFICATION | AVERAGE | |||
---|---|---|---|---|---|
Bulk Density | g/cm3 | Group 26 | 1.0 | ||
Thermal Conductivity | W/mKkcal/moC) | at 350oC JIS R2616 | 0.38 | ||
Cold Crushing Strength | MPa | C93 | 1.5 min | 2.8 | |
Modulus of Rupture | MPa | C93 | 1.5 min | 1.6 | |
Reheat shrinkage | (oC x 8 hrs) | % | C210 JIS R26 13 | 0.5 max | 0.38 (1550oC) |
Thermal Expansion at 1000 oC | % | JIS R26 17 | 0.48 | ||
Chemical analysis | Al2O3 | % | JIS R2216 | 70 | |
Fe2O3 | % | JIS R2216 | 1.0max | 0.7 | |
Mortar | Mortar 1500 | ||||
Standard Packing | 10 pcs / pack for standard size |